Test item |
Unit |
LCK-10 |
Test Methods |
Texture of material |
- |
silica gel+Polyimide film |
- |
Colour |
- |
Yellow |
Visual |
Thickness |
mm | 0.15 |
ASTM D374/374M |
Specific Gravity |
g/cm3 |
1.4 |
ASTM D792 |
Hardness |
Shore A |
90±5 |
ASTM D2240 |
Continuous Use Temp |
℃ |
-60~180 |
- |
Breakdown Voltage |
KV |
≥8.0 |
ASTM D149 |
Volume Resistivity |
Ω·cm |
1014 |
ASTMD257 |
Flame Rating |
- |
V-0 |
UL94 |
Thermal Conductivity |
W/m·K |
1.3 |
ISO 22007-2 |